Meaning
Reduction in volume that occurs as molten metal transitions from a liquid to a solid state must be compensated for by a continuous supply of liquid metal. Solidification shrinkage takes place at the melting point and represents a major source of internal casting defects. Most alloys experience a volume reduction of several percent during this phase change.
Phase Transition
Atoms in the liquid metal arrange themselves into a tight crystalline structure during the freezing process. Crystalline reorganization reduces the average distance between atoms and causes the volume of the metal to shrink. Since this change happens at a constant temperature, it is distinct from the subsequent cooling contraction of the solid metal.
Feeding System
Foundries utilize risers or feeders to supply extra molten metal to the casting as it solidifies. These reservoirs are placed on the heaviest sections of the casting because those areas cool last. By ensuring that the riser remains liquid longer than the main part, the shrinking metal draws liquid from the riser instead of forming an internal cavity.
For complex cast geometries, the design of these risers requires extensive thermal analysis to ensure the feed path remains open until the entire casting is solid.
Defect Prevention
Inadequate compensation for this volume loss leads to shrink holes and spongy porosity in the center of the casting. Such internal cavities compromise the structural integrity of the part and can cause it to fail under pressure. Inspecting critical castings with radiography or ultrasound detects these internal void zones before the parts are shipped.