Meaning
Ratio measurements comparing fluid viscosity at low shear rates to viscosity at high shear rates characterize shear-thinning behavior in chemical formulations. Determination of the thixotropic index indicates how solder paste flows under squeegee shear and recovers structure after deposition. This mathematical ratio governs paste pumpability, aperture filling behavior, and deposit shape retention following stencil release.
Its measurement boundary stops at non-shear fluid dynamics, where static storage temperature alone controls material viscosity.
Viscosity Ratio
Standard rotational viscometers measure fluid resistance at two distinct rotational speeds, typically zero point five revolutions per minute and five revolutions per minute. Calculating the thixotropic index involves dividing the low-speed viscosity value by the high-speed viscosity value. A higher index number indicates a material that thins rapidly under mechanical work but regains high viscosity quickly when shear stress ceases.
Paste formulations designed for surface mount assembly target an index value between one point eight and two point five to balance printability with slump resistance.
Rheological Recovery
Squeegee motion forces paste through stencil apertures by applying high shear rates that drop material viscosity. Once inside the aperture and resting on the PCB pad, the thixotropic index governs how fast internal gel networks rebuild to prevent deposit sagging. Rapid viscosity recovery prevents solder bridging across fine-pitch conductor traces prior to component placement.
Rheological Boundary
Excessive shear exposure over extended print runs breaks down internal polymer binder chains permanently. The thixotropic index fails to predict material behavior when continuous mechanical working degrades the paste vehicle past its elastic recovery point.