Meaning
Corrosion-resistant pre-hardened martensitic stainless tool steel defined by European material standards provides structural mould plates with resistance against acidic resin off-gassing and cooling channel corrosion. Formally designated as din 1.2085 and alloyed with approximately 16 percent chromium and an intentional addition of sulfur, this grade achieves reliable machinability within a delivered hardness range of 280 to 325 HB. The standard governs supply criteria for mould bases, cavity retainers and support plates, halting its authority where high optical polishability is demanded due to micro-voids created by manganese sulfide inclusions.
Corrosive Resistance
Water channel durability eliminates the need for nickel plating inside internal cooling circuits. Plates manufactured from din 1.2085 withstand moisture condensing on chilled mould plates during humid production shifts. Off-gassing from flame-retardant polymers or halogenated resins causes minimal surface pitting on exposed bolster faces.
Rust formation within blind cooling channels remains suppressed over years of continuous water circulation.
Fabrication Behavior
Added sulfur imparts high chip-breaking capability during heavy milling operations. Deep gun-drilling runs true without premature drill wander or tool seizure. Internal sulfide stringers limit surface finishing to technical graining or rough spark erosion.
Optical mirror finishes cannot be achieved because sulfide particles tear from the steel matrix during diamond lapping.
Qualification Benchmark
Verification testing requires material test reports according to DIN EN 10204 type 3.1 certifying sulfur concentration between 0.05 and 0.10 percent and chromium above 15 percent. Hardness across delivery cross-sections must show no variance exceeding 25 Brinell points between exterior surfaces and plate cores. Ultrasonic inspection per ASTM A388 class PL4 confirms absence of internal delamination along rolled directions.
Tool bolsters undergo coordinate inspection after deep milling to confirm that residual stress relief annealing is not required prior to assembly. Final documentation records cooling circuit flow integrity under pressure before the tool enters active moulding cycles. Baseplate flatness ensures stable platen contact under cyclic hydraulic clamp loading.
Thermal expansion coefficients near 10.5 micrometers per meter Kelvin govern thermal gap calculations against standard P20 inserts. Resistance to cooling water fouling preserves cycle times without descaling treatments. Processing PVC-heavy compounds relies on this grade to eliminate secondary bolster corrosion.
Platen contact surfaces resist wash-out caused by ambient condensation in tropical production environments.