Meaning
Spontaneous physical spreading of printed solder paste prior to reflow reduces line resolution and threatens electrical isolation between adjacent circuit pads. Measurement of paste slump evaluates the dimensional instability of printed paste deposits before heating cycles begin. The property governs minimum spacing allowances between solder pads and determines cold and hot slump resistance under standardized test methods.
Boundary conditions stop at the onset of alloy melting, where liquid surface tension takes over deposit shaping.
Viscous Collapse
Internal shear forces and gravitational pull act on the unbaked binder matrix immediately following stencil removal. Resistance to paste slump depends on vehicle thixotropy, metal load percentage, and powder size distribution. High metal load formulations containing fine powder particles offer greater yield strength against lateral spreading.
When binder viscosity drops excessively under shear, paste deposits lose edge definition and sag into inter-pad channels.
Thermal Acceleration
Elevated ambient temperatures in pre-heat zones lower flux vehicle viscosity, accelerating deposit deformation. Laboratory testing for paste slump subjects printed patterns to twenty-five degrees Celsius for cold slump assessment and one hundred fifty degrees Celsius for hot slump assessment. Uncontrolled spreading during warm pre-heat phases bridges narrow gaps between adjacent micro-BGA pads, causing permanent short circuits during reflow.
Bridging Margin
Pad pitch limitations dictate acceptable limits for lateral paste spread across circuit assemblies. Excess paste slump eliminates the clearance gap between neighboring fine-pitch conductors prior to component placement.