Meaning
Pre-hardened chromium-molybdenum alloy steel specified under ASTM A681 designates a standardized mould metal supplied in a heat-treated state between 28 and 32 HRC. This medium-carbon material, formally referenced as aisi p20, balances through-section hardness with machinability for injection tooling and compression dies. Chemical composition centers on 0.35 percent carbon, 1.7 percent chromium and 0.4 percent molybdenum, yielding uniform core strength in heavy cross-sections without secondary hardening.
The specification governs raw billets, pre-machined plates and bolster sets, ending its jurisdiction where surface conversion coatings or secondary nitriding steps alter base mechanical properties.
Core Machinability
Uniform temper permits high metal removal rates with minimal dimensional distortion. Plates of aisi p20 machine cleanly with carbide tooling, avoiding the quench stress cracking common to water-hardening grades. Deep pockets maintain side-wall stability when roughing feeds remain controlled.
Tool wear climbs sharply if the alloy faces high glass-fiber loadings without secondary surface treatments.
Surface Hardening
Gas or ion nitriding raises superficial resistance against abrasive fillers up to 60 HRC. Case depth typically reaches 0.1 to 0.25 millimeters without gross core transformation. Base toughness absorbs mechanical shocks that would crack high-carbon tool steels.
Post-nitriding polishing demands specific stone progressions to avoid fracturing the white layer.
Verification Protocol
Chemical verification via optical emission spectrometry confirms elemental compliance alongside ultrasonic inspection according to ASTM A388 to detect internal voids. Hardness mapping across plate thicknesses identifies center soft spots before pocketing operations commence. Mill test certificates document tensile yield thresholds, which typically exceed 800 megapascals in delivery conditions.
Defective internal soundness risks catastrophic fracture during hydraulic clamping. Mould life projections rely directly on certified initial core hardness. Highly polished lens finishes require vacuum-degassed variants to prevent pitting from non-metallic inclusions.
Final inspection checklists document surface roughness before cavity plating. Correct pre-heating controls reduce welding crack propagation during core modifications. Dimensional stability after pocket hogging remains the primary benchmark for toolmaker acceptance.
Thermal conductivity measures approximately 29 watts per meter Kelvin, guiding conformal cooling line spacing throughout cycling evaluations.