Meaning
Standard specification documents published by the international standards organisation define the chemical composition and mechanical properties of titanium alloy bars. Adhering to the astm b348 standard ensures that milled stock meets the required tensile strength, yield strength and elongation limits before it enters the precision machining phase.
Chemical Requirement
Elemental composition bounds govern the grade of titanium specified for assembly. These limits dictate the maximum allowable levels of iron, carbon, hydrogen, nitrogen and oxygen in the astm b348 material to prevent embrittlement. A low interstitial variant is selected when fracture toughness at cryogenic temperatures is the primary design metric.
In high-stress applications, keeping iron levels below the specified threshhold maintains fatigue resistance during long-term operation.
Product Format
Mill products of various cross-sectional profiles are covered under the scope of this standard. Rectangular, hexagonal and circular geometries machined to astm b348 requirements must undergo non-destructive inspection to detect internal defects before shipping. Traceability is maintained via heat numbers stamped on each individual piece.
Thermal Relief
Thermal treatment sequences are applied to reduce the residual stresses introduced during the rolling or drawing process. Standard annealing profiles for astm b348 titanium prevent distortion during subsequent machining runs. These heat cycles are recorded in the mill test report provided to the purchaser.