Meaning
Sub-micron cavities represent a class of defects that form within solder joints during the reflow process or during subsequent thermal aging. This phenomenon, known as microvoiding, occurs when volatile organic compounds from the solder paste flux are trapped at the interface between the solder and the metal pad. These tiny voids can also develop due to unbalanced diffusion rates between different metals during thermal stress.
They are typically discovered through cross-sectional scanning electron microscopy or high-resolution x-ray imaging.
Kirkendall Effect
Unbalanced interdiffusion at the boundary of copper and tin leads to the formation of empty lattice sites that coalesce into voids. In this context, microvoiding is driven by the Kirkendall effect, where copper atoms diffuse into the solder faster than tin atoms can replace them. This mismatch leaves behind a series of sub-micron holes at the interface of the intermetallic layer.
These holes grow and merge over time, especially when the device operates at high temperatures.
Reliability Impact
Mechanical strength is compromised when a dense band of voids develops along the joint interface. This localized microvoiding makes the joint highly vulnerable to brittle fracture during drop tests. It can also lead to electrical open circuits when the voids connect to form a continuous crack.
Prevention Technique
Solder paste formulation and proper reflow profiles are critical to minimizing the occurrence of these defects. Using paste with lower volatile content and extending the soak time during reflow allows gases to escape before the solder solidifies. This process optimization prevents the gas entrapment that initiates microvoiding.