Meaning
Semiconductor packaging requires protecting delicate silicon chips and wire bonds from mechanical damage and moisture. This packaging method represents transfer molding, which uses a piston to force liquefied thermosetting epoxy into a heated mold cavity. The boundary of the process starts when the assembly is loaded into the mold and ends when the cured package is ejected.
Cycle times are determined by the curing rate.
Material Behavior
Epoxy pellets are preheated to a plastic state before being forced into the runner system. In transfer molding, the resin must have a low viscosity to flow easily around the fine bond wires. After filling the cavities, the epoxy undergoes a chemical reaction that hardens it permanently.
This polymer cross-linking is irreversible.
Tooling Design
Machined steel plates contain multi-cavity designs to maximize output per cycle. Optimizing transfer molding requires runner balancing to ensure that all cavities fill at the same rate. This balancing prevents some packages from under-filling while others are over-compressed.
Heated platens maintain the correct temperature.
Defect Mitigation
Air pockets and incomplete fills reduce the protective value of the package. Improper transfer molding parameters can cause wire sweep, where the flow of epoxy bends the gold wires until they short-circuit. Controlling the injection speed prevents this mechanical displacement of the wire.
High quality requires precise speed control.