Meaning
Copper-tin intermetallic compounds are crystalline structures that form at the boundary between a copper substrate and a tin-based solder. The specific phase identified as cu6sn5 grows rapidly when molten solder contacts the copper pad during reflow. It establishes the mechanical bond that holds the joint together, acting as a bridge between the copper and the bulk solder.
This phase is characterized by a scalloped morphology that can change under subsequent thermal exposure.
Phase Transition
Solid-state diffusion continues to alter the intermetallic layer long after the soldering process has ended. The cu6sn5 phase undergoes a crystal structure change from a hexagonal phase to a monoclinic phase as the joint cools below one hundred and eighty-six degrees Celsius. This transformation causes a volume change of approximately two percent, which can induce micro-cracks in the surrounding solder.
The presence of nickel or cobalt in the solder can suppress this transition and stabilize the hexagonal form.
Growth Control
Thermal aging causes the intermetallic layer to grow thicker over the operating lifetime of the device. If the cu6sn5 layer grows beyond a few micrometers, it can lead to solder joint embrittlement. This growth is accelerated by high operating temperatures, which can cause the joint to fail under mechanical stress.
Nickel Barrier
Preventing excessive copper-tin interaction is often achieved by depositing a nickel barrier layer on the copper pad. This barrier limits the diffusion of copper, resulting in the formation of a nickel-tin intermetallic instead of cu6sn5. This layer is much thinner and more stable, ensuring the long-term reliability of the joint.