Meaning
Thermal conditioning processes remove trapped moisture from plastic surface mount packages before they undergo high temperature soldering. Performing msl 3 baking is necessary for components rated at moisture sensitivity level three to prevent the internal expansion of water vapor. This expansion, known as popcorning, can crack the package or delaminate internal structures during the reflow oven cycle.
The process stops once the component reaches a dry state defined by the J STD 033 standard.
Heat Application
Drying occurs in a specialized oven that maintains a stable temperature, typically 125 degrees Celsius for a set duration. The duration of msl 3 baking depends on the thickness of the package and the amount of moisture it may have absorbed. Components are placed in heat resistant trays to prevent warping or melting.
Handling Requirement
Parts must be processed or resealed in moisture barrier bags immediately after the drying cycle ends. The floor life for a component after msl 3 baking is limited to 168 hours in a controlled environment. If the parts stay out too long, they must repeat the bake cycle.
This adds time to the production schedule and may slightly degrade the solderability of the leads.
Material Integrity
Excessive heating cycles can lead to the growth of intermetallic layers at the lead interface. Limiting the number of times msl 3 baking is performed protects the mechanical strength of the eventual solder joint. Most standards suggest a maximum of two cycles before the component requires additional qualification.
Managing the bake history of every batch is a fundamental part of the quality management system.