Semiconductor manufacturing requires partitioning finished silicon wafers into individual active dies. This physical separation process is saw singulation, which is performed after wafer probe testing is complete. The boundary of the process begins when the wafer is mounted on dicing tape and ends when the diced chips are ready for the assembly pickup tool.
Spindle speed and feed rate must be matched to the wafer thickness to avoid damage.
Blade Selection
Diamond grits embedded in a metal matrix provide the abrasive action needed to cut through hard silicon. During saw singulation, selecting the correct blade thickness is essential to minimize the street width between circuits. Thinner blades reduce material waste but are prone to bending.
The choice depends on wafer layout.
Cooling Action
Friction generates high temperatures at the contact point that can damage the circuitry. Effective saw singulation relies on a continuous flow of deionized water to cool the blade and wash away silicon debris. This rinse prevents thermal stress in the wafer.
Inadequate liquid flow leads to premature blade wear.
Defect Prevention
Chipping along the edges of the die reduces mechanical strength. Controlling saw singulation parameters prevents microcracks from propagating into the active circuitry. Blade wear must be monitored to ensure clean cuts are maintained across the entire batch.
Clean cuts protect die integrity.